The technology of forming a thermite alloy layer on the basis of Fe-Cr-C system on a metal basis by self-propagating high-temperature synthesis is offered, which allows to obtain cast functionallayers withphysico-mechanical and exploitativeproperties. The optimal technological parameters of the forming a wear-resistant layer of thermite alloy process are determined: the amount of metal filler with the maximum yield of suitable alloy, the heating temperature of the thermite charge and the mold to obtain additional heat, the temperature ranges of the melt to melt the metal base with further formation of the functional layer. Metallographic studies of the obtained wear-resistant layer of thermite allo[y showed that the zone of formation of the functional layer is characterized by the stability of the macrostructure and the positive effect of non-metallic inclusions in the form of Al2O3, which influences the formation of chromium carbides in the obtained alloy by creating the effect of inoculative modification of thermite alloy. © Published under licence by IOP Publishing Ltd.

The quest for cost-effective methods to process gold-bearing ores is inextricably linked to a series of preliminary studies, including ore composition analysis, evaluation of the occurrence forms of valuable components, and assessment of the impact of impurity elements and ore physical characteristics on gold recovery. Flotation remains a cornerstone technology in the gold mining industry, essential for the beneficiation of gold-bearing ores. Central to this process is the selection of flotation reagents, which enable effective separation of gold from gangue and associated minerals. This study focuses on the flotation of previously unexamined low-sulfide gold-bearing ore from the Aktobe deposit in the Republic of Kazakhstan. Mineralogical and X-ray phase analyses identified quartz, potassium feldspar, calcite, mica, limonite, and sulfides as the principal minerals in the ore. Phase analysis further revealed that 46.47 % of the gold occurs as free cyanidable gold in open intergrowths, while 37.61 % is locked within sulfides, and 15.92% is finely disseminated in waste rock. To optimize the flotation process, the influence of critical parameters such as grinding size, reagent dosages, flotation time, and flotation machine type on gold recovery was systematically investigated. Closed-circuit tests with one and two cleaner flotation stages were performed using the optimized reagent regime. The results have demonstrated that a single cleaner flotation stage achieved a 1.14 % higher gold recovery, reaching 89.84 %. The concentrate obtained after the cleaner flotation contained 23.01 g/t of gold, making it suitable for subsequent hydrometallurgical processing. © 2024, Ore and Metals Publishing house. All rights reserved.

The article theoretically justified and experimentally confirmed the possibility of implementing the process of the electric melting of Satbayevskiy ilmenite concentrates with new fluxing additives based on oxides and nitrides of aluminium, calcium, and boron. They also include boron carbonitride CNV that will expand the raw material base of Kazakhstan titanium production by involving local substandard material in the process, as well as the technical and economic performance of electric melting. In order to conduct experiments in the area of extremum, the ilmenite concentrate from the Satbayev deposit was taken. Furthermore, the optimum conditions of the electric melting of Satbayevski ilmenite concentrates (such as the process temperature of 1550–1600 °C, the reducing agent consumption of 8–10% of the concentrate mass, and the duration of 90 min), using new fluxing additives, were selected. As a result of the experiment (performed at a temperature of 1600 °C), it has been found that the introduction of 3 to 6% of fluxes in the charge of electric melting promotes the reduction of iron oxides from 45 to 80% and achievement of the extraction of titanium oxide in slag of up to 83.5–90.1%. The addition of 6% boron oxide and carbonitride in the charge of electric melting reduces the melting temperature of the charge to ~1400–1450 °C and the melting time to 90 min. It also creates conditions for a quieter electric melting mode.

This work presents the results of thermodynamic and technological studies of the reducing electric smelting of low-quality and difficult-to-recover Satpaevsk ilmenite concentrates in the presence of sodium carbonate (Na2CO3) as a flux. In the course of thermodynamic studies, according to literature data and using the HSC Chemistry 8 program, the state diagrams of the FeO-TiO2, FeO-Fe2O3-TiO2, Na2O-TiO2, Na2O-SiO2, Ti-C-O and Fe-C-O systems and the possibility of reactions in the temperature range of 500–1600 °C (without smelting of titanium, 1678 °C), taking into account phase transitions, were studied. The article also presents the results of technological studies of the above process. In general, the research results showed the possibility of using sodium carbonate (Na2CO3) as a flux in the charge of the electric smelting of low-quality Satpaevsk ilmenite concentrates. It has been established that the addition of 4.5–5% of Na2CO3 allows for reducing the temperature and the duration of electric smelting, the viscosity of the melt, and the complete separation of the smelting products (cast iron from slag).

As is well known, one of the key problems facing modern humanity is atmospheric pollution caused by harmful industrial emissions, which negatively affect both the environment and public health. The main goal of this study is to conduct an analytical assessment of the impact of atmospheric air pollution on public health, using molybdenum production as an example. The evaluation includes an analysis of the acute toxic effects of pollutants on public health resulting from emissions of a molybdenum enterprise. The assessment of health risks caused by exposure to chemical air pollutants in the emissions of molybdenum mining enterprises revealed that the individual carcinogenic risk associated with substances such as nitrogen dioxide, dust, ammonia, sodium sulfide, and benzo [a] pyrene (a total of 17 substances) is 0.999.

The purpose of the study is to develop and evaluate the effectiveness of an innovative cargo fastening system using aramid fasteners to improve the safety and stability of cargo transportation. The research methodology included the analysis of existing solutions, the development of conceptual models, mathematical calculations, and the modelling of the system using three-dimensional models. In addition, this study paid special attention to the choice of fastening materials, such as aramid fibre, and analysed the strength characteristics of fasteners to ensure maximum safety of cargo transportation. As a result of the work conducted, an innovative cargo and object fixation system was created, which provides a high level of protection and safety for the cargo, allowing it to avoid damage and emergency situations during transportation. Notably, this system is able to effectively distribute the load and reduce the impact of inertial forces, ensuring stability and reliability during the transportation of goods of various types and sizes. An additional substantial advantage of this innovative solution is its versatility, which allows its successful use in various scenarios and conditions. The technical solution created is suitable for moving both light and heavy loads and can be effectively applied to various types of vehicles. Copyright: © 2025 Nadezhda Dolzhenko, Gulnar Imasheva, Assel Berkesheva, Olga Garmash, and Tasbulat Beketov. This article is an open-access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY 4.0) license.

The article presents the results of enrichment of gold-bearing ore from the Aktobe deposit, containing 1.57 g/t of gold, using flotation and gravity–flotation flowsheets with a closed flotation circuit. The expediency of obtaining gold-bearing concentrate by flotation with one cleaner operation is established. The following process indicators are obtained: the yield of the flotation concentrate is 6.13%; the gold content is 23.01 g/t at the recovery of 89.84%. The comparative analysis of the closed-loop flotation circuit results shows that the obtained indicators in both flotation and gravity–flotation flowsheets are approximately at the same level. The highest process indicators in terms of recovery are obtained using the integrated grinding–centrifugal concentration–flotation flowsheet with one cleaner operation. In this case, gold recovery is 90.56%, which is 0.72% higher than the recovery in flotation flowsheet. The studies on gold cyanidation and adsorption at activated carbon grade Gold Curb 207 C demonstrate low gold recovery, both during cyanidation of the original ore (recovery 62.42%) and during cyanidation of the flotation concentrate (recovery 48.53%). To increase the cyanidation efficiency, the methods of concentrate preparation for cyanidation such as pyrometallurgical treatment (roasting) and mechanical activation (ultrafine grinding) are recommended. © 2025, Ore and Metals Publishing house. All rights reserved.
The study considered ore enrichment waste from the Ashiktas, Akbakai, and Maikain deposits to create sorbents based on silicophosphates. X-ray phase and electron probe elemental analysis were carried out, which confirmed the presence of silicon, aluminosilicate, and other valuable components suitable for the sorbents synthesis. The optimal synthesis temperature (600°C) contributes to the sorbents' porous structure development and a sorption capacity increase concerning Ni2+ ions, allowing them to be used to purify industrial wastewater from heavy metals, which was proven using zeta potential measurements and SEM images.

Extraction of gold from refractory gold-bearing ores in processing with combined flow charts is higher if more gold is extracted by gravity methods before flotation and hydrometallurgical circuits. The article presents the results of gravity beneficiation of refractory gold-bearing ore from the Aktobe deposit with the cyanidation-recoverable gold content of 46.47%. Assessment of the gravity separation efficiency used the GRG-test which found that 35.93% of gold could be extracted in centrifugal concentration. Two flow charts of gravity concentration of ore in the grinding circuits with jigging and centrifugal concentration were tested. The studies find out that the main amount of Aktobe gold has a size less than 0.1 mm, and it is recommended to recover such gold by combining grinding and centrifugal concentration in the integrated processing circuit. © 2024, Ore and Metals Publishing house. All rights reserved.
The properties of phosphate coatings formed on St3 carbon steel were investigated using calcium–manganese–phosphate solutions derived from Zhayrem ore beneficiation wastes and compared with conventional Mazhef salt solutions. Protective performance was evaluated using the drop method, gravimetric tests, and electrochemical techniques. Coatings obtained from the waste-derived solution at 85 °C for 60 minutes exhibited a protective capacity 1.5 times higher than those formed in Mazhef solutions. Electrochemical measurements confirmed this result, with corrosion current densities of 0.974 µA/cm2 for waste-derived coatings, compared to 1.623 µA/cm2 for Mazhef coatings and 2.337 µA/cm2 for uncoated steel. Gravimetric tests showed a lower mass loss over 8 days of immersion (0.0024 g vs. 0.0058 g). SEM and EDS analyses revealed that waste-derived coatings formed dense Ca–Fe–Mn–P layers with a thickness of ~11.1 µm, while Mazhef coatings were thinner (2.96–6.23 µm) and more porous. These findings demonstrate that manganese ore beneficiation wastes are an effective and sustainable source of phosphating agents for producing corrosion-resistant coatings on carbon steel.